Negotiable
The date of payment from buyers deliver within days
Beijing
Long-term effective
2017-09-12 05:37
320
Company Profile
By certification [File Integrity]
Contact:runhe(Mr.)
Email:
Telephone:
Phone:
Area:Beijing
Address:Room 1906, Guangli Mansion, 136# Qingchun Road, Hangzhou, China
Website:http://www.runhesilicone.com/ http://runhe.shxghby.com/
Within those famous super smooth amino silicone oil rh-nb-8010 manufacturers and suppliers in China, RUNHE is the most reliable. You are welcomed to wholesale low price super smooth amino silicone oil rh-nb-8010 from our factory and check the quotation with us.
Super Smooth and Clear Silicone Oil RH-NB-8010
【Product Name】Super Smooth and Clear Silicone Oil RH-NB-8010
【Introduction】 It is a modified polysiloxane
【Advantage】 Very smooth and clear hand feeling.
【Basic Character】
Appearance: Colorless to tiny yellow transparent liquid
Ionic:weak-cation
Amino Value: 0.10-0.20mmol/g
Viscosity: 10000~40000mpa•s
【Application】
Applied for the smooth and clear finishing of cotton,viscose,tencl and Cellulose Fibers.
【Usage amount for reference 】
Crude oil emulsification please refer to the emulsification process.
(1)Dipping Process: Dilution 1~5 %( o.w.f)
(2)Padding Process: Dilution 10~40g/l
【Package】50 or 120kg/drum
【Storage】Store in cool and ventilated warehouse. 6 moths of storage period.
Emulsification Process
Formulation
1.RH-NB-8010 20KG
2.Emulsifier 10KG
3.Glacial acetic acid 1.5kg+3.5kg water 5Kg
4. Water 65KG
Diluted into 30% amino silicone emulsion.
Process
(1).Add RH-NB-8010 and the emulsifier in the container, and start to stir for 5-10min.
(2).Add 4Kg water and stir for 5minutes, the add 0.5kg acetic water ,stir 5-10min.
(3).Add 4Kg water and stir for 5minutes, the add 0.5kg acetic water ,stir 5-10min.
(4).Add 4Kg water and stir for 5minutes, the add 0.5kg acetic water ,stir 5-10min.
(5).Add 8Kg water and stir for 5minutes, the add 0.5kg acetic water ,stir 5-10min.
(6).Add 15Kg water and stir for 5minutes, the add 1kg acetic water ,stir 5-10min.
(7).Add 15Kg water and stir for 5minutes, the add 2kg acetic water ,stir 5-10min.
(8).Add 15kg water stir for 10min,can add some glacial acetic acid make the pH at 6.filtering and packaging